Congratulations on starting this page. However I would like to comment about your defintion and description of dunting: this is a fault that results from thermal shock following rapid change in temperature, most commonly on coolling, and not due to body - glaze mismatch. Before editing your text I thought it only polite to enter something on the discussion pages

Oh, you will have seen that I've change clay to clay body, or just body, in the entry to better describe the material

Regards,

Andy


Hi Guys. Ive added a 'This article or section is in need of attention from an expert on the subject.'to flag correction is needed on the errors


Description edit

I've done a little bit on the article, correcting that on dunting, but the crazing and shivering still needes improving, for example the description should refernce thermal expansion more than it does at presentTheriac 13:38, 8 January 2007 (UTC)Reply

Did a tiny bit more. Still lots to do. Have flagged a dubious / incorrect / over simplified description. ThanxTheriac 08:20, 7 February 2007 (UTC)Reply